Contact SupplierStir the coating thoroughly before application
Take out requisite quantity of Craftanol-256 IP; if required dilute the coating by CRAFTANOL THINNER to desired degree of consistency as per application practice.
Brushing:- Ready For Use(After thorough mixing)
Apply the coating by brushing.
Ignite the coating immediately after applying. In case of large moulds part mould to be coated & ignited immediately.Craftanol- 256 IP is recommended for high temperature metals like Steels, Alloy Steels, heavy section cast irons and for copper base alloys. High temperature metals heavy section cast iron precision cast iron casting requires high temperature coating barriers which can withstand high metallostatic pressure of liquid metal to prevent Sand fusion other problems related to Sand and to improve the surface finish of Casting.