Phosphate coating weight for wire drawing is usually in the range of 5-15 g/m². It is a fine and homogeneous coating that should be considered here. If the coating on the wire is not fine crystalline or homogeneous, activation should be used before the phosphate bath. With the use of activation, a thinner, dense and smoother coating is obtained and coating continuity is provided for multiple drawings