Listing ID #5787411
Company Information
Ask for more detail from the seller
Contact SupplierChemical Composition of Deposited Metal (%):
C | Si | Mn | S | P |
≤0.18 | ≤0.90 | ≤1.75 | ≤0.030 | ≤0.030 |
Mechanical Property of Deposited Metal:
Tensile Strength MPa |
Yield Strength MPa |
Elongation Rate (%) |
Test Temperature °C |
Akv Impact Value (J) |
≥490 | ≥400 | ≥22 | -20 | ≥47 |
The Diameter and Reference Current of Welding Wire:
Diameter (mm) |
φ1.2 | φ1.4 | φ1.6 |
Current (A) |
120~300 | 150~400 | 180~450 |