Contact SupplierThe company is enlisted among the topmost Manufacturers, Exporters and Suppliers of SS317L Stainless Steel Products. Our products are fabricated using superior grade stainless steel and advanced machines to ensure excellent quality and perfect finish. Our products have wide application in numerous industries and we offer them in required specifications. Buyers can place bulk as well as urgent orders with us!
General Properties : Alloy 317L is molybdenum-bearing austenitic stainless steels with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless steels such as Alloy 304. In addition, 317L alloys offer higher creep, stress-to-rupture, and tensile strengths at elevated temperatures than conventional stainless steels. All are low carbon or "L" grades to provide resistance to sensitization during welding and other thermal processes. The combination of molybdenum and nitrogen is particularly effective in enhancing resistance to pitting and crevice corrosion, especially in process streams containing acids, chlorides, and sulfur compounds at elevated temperatures. Nitrogen also serves to increase the strength of these alloys. Both alloys are intended for severe service conditions such as flue gas desulfurization (FGD) systems.
Resistance to Corrosion :
Physical Properties : The physical property data which follows represent the iron-chromium-nickel-molybdenum class of stainless steels. For all practical purposes, the data are applicable to Alloy 317L stainless steel. All properties are at room temperature (68°F, 20°C) unless stated otherwise.
Density lbM/in3 | Modulus of Elasticity | Melting Range | Thermal Conductivity Btu/ft2-hr-oF-in | 68 to 212oF Watts/m- K | 212oF (100oC) 10-6/oF (10-6/oC) | 932oF (500oC) | 1832oF (1000oC) | Specific Heat | Electrical Resistivity | Magnetic Permeability | Fully annealed µ at H = 200 oe | |||||
g/cm3 | psi | Gpa | oF | oC | Btu/lb-oF | J/g-oK | µ-ohm-in | µ-ohm-in | ||||||||
0.29 | 8 | 29•106 | 200 | 2410 to 2550 | 1320 to 1400 | 100.8 | 14.6 | 10.8 (19.5) | - | - | 0.11 | 0.46 | 31.1 | 0.79 | - | 1 |
Minimum Mechanical Properties per | ||||||
ASTM A-240 for Cited Alloys | ||||||
Property | Ultimate Tensile Strength, ksi (MPa) | 0.2% Yield Strength, ksi (MPa) | % Elongation in 2" (5.1 cm) | |||
Alloy 317L | 75 | -515 | 30 | -205 | 40 |
Crevice Corrosion in a Simulated | FGD System Environment | Alloy | Alloy 317L | Alloy 625 | Alloy C276 | |||
---|---|---|---|---|---|---|---|---|
Weight Loss (g/cm2) | for Tests* at Cited Temperatures | 24oC | (75oF) | 0 | 0 | 0 | ||
- | - | - | - | 50oC | (122oF) | 0.04 | 0 | 0 |
- | - | - | - | 70oC | (158oF) | 0.05 | 0.01 | 0 |
Pitting Resistance Equivalents | Alloy | Alloy 316 | Alloy 317L | Alloy 625 | Alloy C276 |
---|---|---|---|---|---|
PRE | 25 | 30 | 52 | 69 |