Contact SupplierWe are reckoned as one of the foremost Manufacturers of PVC Stabilizer in the country. In PVC Processing (extrusion, injection moulding etc.), the polymer is subjected to high temperature which can lead to burning )degradation or breaking of polymer chains). Heat stablizers are lead compounds that are added to prevent burning.
Conventionally combination of three chemicals, TBLS, DBLS and LS (Tribasic lead sulphate, dibasic Lead stearate and Lead stearate) were used as heat stablizers with Calcium Stearate as a co-stablizer. Now one pack is used in place of the three chemicals as heat stabilizer. Its performance depens on two things
PROPERTY | UNIT | PP-2 | PP-3 | PP-4 |
---|---|---|---|---|
Appearance | ------- | Snow White free flowing powder | ||
Metal Content | % | 30-35 | 35-40 | 50-55 |
Specific Gravity | ------- | 2.2-2.4 | 2.3-2.4 | 2.4-2.5 |
Moisture | % max | 0.5 | 0.5 | 0.5 |
pH | ------- | 6.5-7.5 | 6.5-7.5 | 6.5-7.5 |
Melting Point | oC | 105-110 | 105-110 | 105-110 |
Residue on 240 mesh | % max | 0.5 | 0.5 | 0.5 |
Free fatty matter | % max | 0.2 | 0.2 | 0.2 |
PROPERTY | UNIT | PP-2 | PP-3 | PP-4 |
---|---|---|---|---|
Appearance | ------- | Snow White free flowing powder | ||
Metal Content | % | 30-35 | 40-45 | 50-55 |
Specific Gravity | ------- | 2.2-2.4 | 2.3-2.4 | 2.4-2.5 |
Moisture | % max | 0.5 | 0.5 | 0.5 |
pH | ------- | 6.5-7.5 | 6.5-7.5 | 6.5-7.5 |
Melting Point | oC | 105-110 | 105-110 | 105-110 |
Residue on 240 mesh | % max | 0.5 | 0.5 | 0.5 |
Free fatty matter | % max | 0.2 | 0.2 | 0.2 |