Listing ID #3888782
Company Information
Ask for more detail from the seller
Contact SupplierNatural Reclaim Rubber recycled out from natural rubber tube scrap with well equipped and modernized machinery. Today the use of natural reclaim rubber is widespread, ranging from household to industrial product
Application:Chemical Index | ||
RNRR-111 | ||
Test Name | Test Method | Content |
Ash Content (%) | ASTM D297-18 | 30 Max. |
Carbon Black (%) | ASTM E1131 | 20 – 27 |
Acetone Extract (%) | ASTM D297-18 | 9 - 15 |
Volatile Matter (%) | 1% Max | |
RHC (%) | ASTM E1131 | 42 Min. |
Physical Index | ||
Test Name | Test Method | Content |
Specific Gravity (gm/cc) | ASTM D297-18 | 1.30 Max. |
Tensile Strength (kg/cm²) | ASTM D412 | 30 Min. |
Elogation At Break (%) | ASTM D412 | 250 Min. |
Mooney Viscosity (ml) | ASTM D1646 | 35 - 55 |
Hardness (Shore A) | ASTM 2240 | 50 - 60 |