Contact SupplierStandard | Before Agening | Temperature of Ageing Degree C | Duration of Ageing hrs | After Ageing | ||||
Tensile Strength Mpa | Elongation % | Tensile Strength Mpa | Elongation % | Maximum Abrasion loss MM | ||||
GRADE HR (T-1) IS1981 Part-1 | ||||||||
This grade is recommended for conveying hot material and is suitable for fines upto 100°c and coarse material upto 125°C | 12.5 | 350 | 350 | 100 | -25 | -40 | 200 | |
GRADE HR (T-2) IS1981 Part-2 | ||||||||
This grade is recommended for conveying hot material and suitable for lines upto 125°C and lumps upto 150°C | 12.5 | 350 | 125 | 72 | -35 | -50 | 250 |