Contact SupplierWe are manufacturing a wide range of filter papers & pads on a very highly sophisticated production plant. The entire process of manufacturing is untouched by hand from the pulping stage to the finished product. This is a high precision completely automatic plant which ensures a uniformly produced filter media for excellent purity and frees from external contaminants qualities vital for sensitive industries like drugs, pharmaceuticals, foods, beverages, chemicals,cosmetics etc.
Our raw material is continuously monitored for quality control.Constant laboratory tests are conducted to check filtration efficiency,pad porosity, absorbency, Filteration speed and bursting factor. The fibers of our filter paper & pads are also subjected to a special porous chemically inert wet-strength impregnation process to impart very high mechanical strength while filtering aqueous.
We also manufacture handmade filter papers & pads as per customer’s requirement. We use pure Cellulose Fibre, Cotton linter Pulp in manufacturing Quality filter Papers
The raw material used in manufacturing this grade of filter pad is 100% cellulose Cotton pulp which is unbleached. The pad is manufactured and continuously monitored under the rules of food act so it can be used to filter any food grade liquid.
This is Non-Toxic, Non-Explosive, Non-Corrossive, Non- flammable And Non Hazardous/Dangerous, Dust free.
Keep it in a dry place.
FILTER PAD TESTING PARAMETERSGRADE | THICKNESS | G.S.M | POROSITY | MAX. PORE SIZE | B.F | BULK |
---|---|---|---|---|---|---|
MMC-05 | 0.5mm | 250gsm. | 4to5sec | 3µ | 3kg/cm2 | 0.002 gm/cc |
MMC-1 | 1mm | 500gsm | 6to7sec | 4µ | 5kg/cm2 | 0.002 gm/cc |
SW-1 | 1.2mm | 900gsm. | 120sec. | 1µ | 10kg/cm2 | 0.011 gm/cc |
MMCR-05 | 0.5mm | 300gsm | 4to5sec | 3 µ | 4/cm2 | 0.016 gm/cc |
MMCR-1 | 1mm | 500gsm | 5sec | 3 µ | 4kg/cm2 | 0.002 gm/cc |
MMCR-15 | 1.5mm | 650 gsm. | 7 Sec. | 4µto5µ. | 7Kg./cm2 | 0.025 gm/cc |
MMCR-2 | 2mm | 800gsm | 8 Sec. | 5 µ | 9 Kg/ cm2 | 0.033 gm/cc |
MMCR-25 | 2.5mm | 1100gsm. | 8 Sec. | 2to3 µ | 10kg/cm2 | 0.022 gm/cc |
MMCR-3 | 3mm | 1300gsm. | 10sec. | 3 to5 µ | 10kg./cm2 | 0.023 gm/cc |
KL-2 | 2mm | 800gsm | 3sec. | 30 µ | 5Kg/cm2 | 0.025 gm/cc |
KL-25 | 2.5mm | 1100gsm | 4to5sec. | 25 µ | 6kg/cm2 | 0.022 gm/cc |
KL-3 | 3mm | 1250gsm | 5to6sec | 20 µ | 8/cm2 | 0.024 gm/cc |
Kl-35 | 3.5mm | 1400gsm | 5to6 sec | 35 µ | 10kg/cm2 | 0.025 gm/cc |