Contact SupplierProperty | Units | Results | Test method (ASTM) |
Specific Gravity | 1.19 | D 792-60 T | |
Optical | |||
Refractive lndex | 1.49 | D 542-50 | |
Light Transmittance | D 1003-61 | ||
‧Parallel | % | 92 | |
‧Total | % | 93 | |
‧Haze | % | 1 | |
Mechanical | |||
Tensile Strength | D 638-61T | ||
‧Rupture | kg/c㎡ | 760 | |
‧Modulus of Elasticity | kg/c㎡ | 30000 | |
‧Elongation | % | 4.5 | |
Flexual Strength | D 790-63 | ||
‧Rupture | kg/c㎡ | 1050 | |
‧Modulus of Elasticity | kg/c㎡ | 30000 | |
Compressive Strength | D 695-63 T | ||
‧Yield | kg/c㎡ | 1260 | |
‧Modulus of Elasticity | kg/c㎡ | 30000 | |
Shear Strength | kg/c㎡ | 630 | D 732-46 |
Impact Strength | D 256-56 | ||
‧Izod Milled Notch(200 gr.steel ball) | m | 0.4 | |
Rock Well Hardness | M100 | D 785-62 | |
Thermal | |||
Hot Forming Temperature | ℃ | 140-180 | D 648-56 |
Heat Distortion Temperature 2℃ /min-264 p.s.i | ℃ | 85 | |
Maximum Recommended Continuous Srve Temperature | ℃ | 85 | |
Coefficient of Thermal Conductivity | Cal/cmsec.℃ | 0.0006 | D 696-44 |
Coefficient of Thermal Linear Expansion | cm/cm.℃ | 0.00007 | |
Specific Heat | Cal/gr℃ | 0.35 | |
Electrical | |||
Surface Resistivity 28℃,75%RH | ohmh | >1016 | |
Volume Resistivity | ohmh.cm | >1015 | D 257-61 |
Dielectric Strength Shot Time Test(0.125 sec.) | kv/cm | 160 | D 149-64 |
Arc Resistance | No Track | D 495-61 | |
Miscellaneous | |||
Flammability | mm/min | 33 | D 635-63 |
Water Absorption | |||
‧Wt.Gain on Immersion for 24hrs | % | 0.3 | D 570-63 |
Odor | None | ||
Taste | None |