Product Name | Element Analysis | ||||
---|---|---|---|---|---|
GO-GRAPHENE OXIDE | C(%) | O(%) | S(%) | H(%) | N(%) |
72.5 | 45 | 0.4 | 1.2 | 4.9 | |
PARAMETERS | APPROXIMATE VALUES | ||||
Thickness | 0.8 ~ 2 nm | ||||
Carbon Purity | ~99% | ||||
Number of Layers | Average number of layers 1-3 | ||||
Surface Area (BET) | >120 m2/g | ||||
Bulk density | 0.4 g/cc | ||||
Electrical Conductivity | Insulator [Tuneable to conductor] | ||||
Lateral dimension | 5-10 μm |